| Xtel® XE5300NA is a high performance extrusion grade PPS based alloy developed to provide excellent mechanical strength, elongation and chemical resistance. |
|
| NOMINAL ENGINEERING PROPERTIES(1) |
Value |
Test Method |
| Tensile Strength, psi |
8000 |
ASTM D638 |
| Elongation, % |
12 |
ASTM D638 |
| Flexural Strength, psi |
14,000 |
ASTM D790 |
| Flexural Modulus, psi |
350,000 |
ASTM D790 |
| Elastic Modulus, psi |
320,000 |
ASTM D638 |
| Notched Izod Impact, ft·lb/in, 1/8 in specimen |
1.0 |
ASTM D256 |
| Heat Deflection Temperature, 264 psi,°F |
195 |
ASTM D648 |
| Heat Deflection Temperature, 66 psi,°F |
265 |
ASTM D648 |
| Coefficient of Linear Thermal Exp., X 10-6 in/in/°C |
  |
ASTM E831 |
| Axial Direction, -50°C to 50°C |
70 |
  |
| Axial Direction, 100°C to 200°C |
125 |
  |
| Transverse Direction, -50°C to 50°C |
70 |
  |
| Transverse Direction, 100°C to 200°C |
125 |
  |
| Flammability Rating |
V-0(2) |
UL 94 |
| Thermal Conductivity, BTU·in/hr·ft2·°F |
1.4 |
  |
| Dielectric Strength, V/mil |
600 |
ASTM D149 |
| Dielectric Constant, 78° F |
|
ASTM D150 |
| 1kHz |
3.3 |
  |
| 1MHz |
3.3 |
  |
| Dissipation Factor, 78°F |
|
ASTM D150 |
| 1 kHz |
0.006 |
|
| 1 MHz |
0.009 |
|
| Volume Resistivity, ohm·cm |
1 x 1015 |
ASTM D257 |
| Comparative Tracking Index, V |
125(2) |
UL 746A |
| Density, g/cc |
1.30 |
ASTM D792 |
| Water Absorption, % |
0.10 |
ASTM D570 |
| Color |
Natural |
  |
|
| (1) Test specimen molding conditions: Stock Temperature, 600-650°F; Mold Temperature, 275°F |
| (2) This product is not currently UL Listed; test results indicate this level of performance |
| The nominal properties reported herein are typical of the product but do not reflect normal testing variances and therefore should not be used for specification purposes. |
| Xtel® XE5300NA is a high performance extrusion grade PPS based alloy developed to provide excellent mechanical strength, elongation and chemical resistance. |
|
| NOMINAL ENGINEERING PROPERTIES(5) |
Value |
Test Method |
| Tensile Strength, MPa |
55 |
ISO 527 |
| Elongation, % |
12 |
ISO 527 |
| Flexural Strength, MPa |
95 |
ISO 178 |
| Flexural Modulus, MPa |
2500 |
ISO 178 |
| Elastic Modulus, MPa |
2200 |
ISO 527 |
| Notched Izod Impact, kJ/m2 |
6.0 |
ISO 180A |
| Heat Deflection Temperature, 1.8 MPa,°C |
90 |
ISO 75 |
| Heat Deflection Temperature, 0.45 MPa,°C |
130 |
ISO 75 |
| Coefficient of Linear Thermal Exp., X 10-6 in/in/°C |
  |
ISO 11359-2 |
| Axial Direction, -50°C to 50°C |
70 |
|
| Axial Direction, 100°C to 200°C |
125 |
|
| Transverse Direction, -50°C to 50°C |
70 |
|
| Transverse Direction, 100°C to 200°C |
125 |
  |
| Flammability Rating |
V-0(6) |
UL 94 |
| Thermal Conductivity, W/m·K |
0.20 |
  |
| Dielectric Strength, kV/mm |
24 |
ASTM D149 |
| Dielectric Constant, 25°C |
|
ASTM D150 |
| 1kHz |
3.3 |
|
| 1MHz |
3.3 |
|
| Dissipation Factor, 25°C |
  |
ASTM D150 |
| 1 kHz |
0.006 |
|
| 1 MHz |
0.009 |
|
| Volume Resistivity, ohm·cm |
1 x 1015 |
ASTM D257 |
| Comparative Tracking Index, V |
125(6) |
UL 746A |
| Density, g/cc |
1.30 |
ISO 1183A |
| Water Absorption, % |
0.10 |
ASTM D570 |
| Color |
Natural |
  |
|
| (5) Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C |
| (6) This product is not currently UL Listed; test results indicate this level of performance |
| The nominal properties reported herein are typical of the product but do not reflect normal testing variances and therefore should not be used for specification purposes. |
|
|