| This linear low density, high molecular weight hexene copolymer is tailored for sheet and geomembrane applications that require: |
|
| Typical geomembrane applications for 7104 include: |
|
|
| Typical sheet applications for 7104 include: |
|
| This resin meets these specifications: |
|
| NOMINAL PHYSICAL PROPERTIES (1) |
English |
SI |
Method |
| Density |
--- |
0.919 g/cm3 |
ASTM D1505 |
| Melt Index, 190/2.16 |
--- |
0.35 g/10 min |
ASTM D1238 |
| Tensile Strength at Yield, 2 in/min, Type IV bar |
1,600 psi |
11 MPa |
ASTM D638 |
| Elongation at Break, 2 in/min, Type IV bar |
700% |
700% |
ASTM D638 |
| Flexural Modulus, Tangent - 16:1 span:depth, 0.5 in/min |
60,000 psi |
410 MPa |
ASTM D790 |
| ESCR, Condition B (10% Igepal), F50 |
>2,000 h |
>2,000 h |
ASTM D1693 |
| ESCR, Condition C (100% Igepal), F50 |
>2,000 h |
>2,000 h |
ASTM D1693 |
| SP-NCTL |
>1,000 h |
>1,000 h |
ASTM D5397 (Appendix) |
| Durometer Hardness, Type D (Shore D) |
51 |
51 |
ASTM D2240 |
| Vicat Softening Temperature, Loading 1, Rate A |
212°F |
100°C |
ASTM D1525 |
| Heat Deflection Temperature, 66 psi, Method A |
123°F |
51°C |
ASTM D648 |
| Brittleness Temperature, Type A, Type I specimen |
<-103°F |
<-75°C |
ASTM D746 |
| Oxidative Induction Time, 200°C |
>100 min |
>100 min |
ASTM D3895 |
-
The nominal properties reported herein are typical of the product, but do not reflect normal testing variance and therefore should not be used for specification purposes. Values are rounded. The physical properties were determined on compression molded specimens that were prepared in accordance with Procedure C of ASTM D4703, Annex A1.
|
|
|